Development and Applications of Multi-physics Coupled Numerical Model for Friction Stir Welding

Researchers at Oak Ridge National Laboratory developed a model to study friction, heat generation, heat transfer and material flow during the friction stir welding process. The numerical simulation may advance the design of FSW tools and the optimization of FSW parameters.