Evaluation of HAZ Hydrogen-induced Cracking for High Strength Steels

Evaluation of HAZ Hydrogen-induced Cracking for High Strength Steels

Researchers use the implant test to investigate the susceptibility of high strength steels to hydrogen induced cracking of the heat affected zone.