A Local-to-Global Assembling Method to Predict Distortion

A Local-to-Global Assembling Method to Predict Distortion

This presentation introduces the development of the local-to-global assembling method, the implementation of this method to commercial software, and the application of this method to predict distortion in larger welded structures.