EXPERIMENTAL DEVELOPMENT FOR THERMAL MEASUREMENTS OF RAPID AM SOLIDIFICATION
Ailsa Craigmile
SIGMA FORMATION IN 2707 STAINLESS STEEL
Evan Freeland
SIX ESSENTIALS OF SHIELDED METAL ARC WELDING (SMAW)
Luke Wilson
Category C
COMPUTATION OF PSEUDO-BINARY PHASE DIAGRAMS FOR DISSIMILAR METAL WELDS
Ryan Lannutti
HIGH SPEED VIDEO CAPTURE OF RESISTANCE SPOT WELDING
Chris Dugan
CORROSION RESISTANT WELD OVERLAYS FOR PIPELINES, OIL AND GAS, AND PETROCHEMICAL INSTALLATIONS
Timothy Babyak
Category D
CORRELATION OF PHYSICAL AND NUMERICAL SIMULATIONS OF DDC IN MULTIPASS WELDS
Samuel Luther
REACTION SYNTHESIS FEEDSTOCKS FOR ADDITIVE MANUFACTURING
Ethan Sullivan
SIMULATED HEAT AFFECTED ZONES COMPARED TO TOUGHNESS AND MICROSTRUCTURE IN CARBON STEEL WELDS
Kaleb Gabbert
2019 POSTER WINNERS
Category A
EFFECTS OF WIRE FEED SPEED ON WELDS
Mallory Hallwirth
HISTORY OF WELDING
Emerson T. Severt
EFFECTS OF GAS MIXTURES (GTAW)
Hunter Beckett
Category B
THE IMPORTANCE OF PROPER USE OF RESPIRATION AND VENTILATION IN WELDING
Ryan Turley
Category C
EVALUATION OF F22 HAZ HARDNESS AND TEMPERING RESPONSE
Griffin Goldenbagen
EVALUATION OF DISSIMILAR STAINLESS STEEL WELDS FOR FUEL PUMP APPLICATIONS
Corey Cox
MICRO-RESISTANCE WELDING FOR MEDICAL APPLICATIONS
Luke Walker
Category D
WELDABILITY OPTIMIZATION OF NICKEL BASE ALLOYS VIA MODELING AND ADVANCED CHARACTERIZATION
Allison Fraser
SOLIDIFICATION BEHAVIOR OF HIGH-ENTROPY ALLOY FILLER DURING BRAZING OF NI-BASE SUPERALLOY
Benjamin Schneiderman
MICROSTRUCTURAL CHARACTERIZATION AND MECHANICAL PROPERTY EVALUATION OF A NOVEL 10 wt% Ni STELL WELDING CONSUMABLE
Erin Barrick
Category E
CONTROL OF WELD RESIDUAL STRESS THROUGH LOW TRANSFORMATION TEMPERATURE WELDING CONSUMABLES
Xin Wu
2018 POSTER WINNERS
Category A
WELDING – STICK, TIG & MIG
Cameron Wenclewicz
EFFECTS OF POLARITY ON PENETRATION AND CLEANING
Kyle Kinder
GAS METAL ARC WELDING (GMAW)
Dylan Vanderpool
Category C
WELDABILITY OF DISSIMILAR STAINLESS STEELS FOR FUEL PUMP APPLICATIONS
Alvin Kirksey
LIQUID METAL EMBRITTLEMENT IN RESISTANCE SPOT WELDS OF ADVANCED HIGH STRENGTH STEELS: MICROSTRUCTURE AND FRACTURE CHARACTERISTIC
Michael Stotts
MICROSTRUCTURAL EVOLUTION OF DISSIMILAR METAL WELDS INVOLVING GRADE 91 STEEL
Michelle Kent
Category D
A SCANNING TRANSMISSION ELECTRON MICROSCOPY STUDY OF THE HEAT-AFFECTED ZONE IN 10 wt% Ni STEEL WELDS
Erin Barrick
DYNAMIC LASER WELDING BEHAVIOR OF WROUGHT AND ADDITIVE MANUFACTURING STAINLESS STEELS
Cheryl Hawk
EFFECT OF ALLOYING ELEMENTS ON THE WELDABILITY OF NICKEL BASE ALLOYS
Allison Fraser
Category E
FORMATION OF DELTA FERRITE IN THE HAZ OF GRADE 91 DISSIMILAR METAL WELDS
Mike Kuper
QUALITY PREDICTION OF RESISTANCE SPOT WELDING USING DEEP NEURAL NETWORK ALGORITHM
In-sung Hwang
DEVELOPMENT OF CONSUMABLES AND WET WELDING PROCEDURES AIMING CLASS A STRUCTURAL REPAIRS IN SHALLOW WATERS FLOATING PRODUCTION UNITS
Ezequiel Caires Pereira Pessoa
2017 POSTER WINNERS
Category B
EFFECT OF POLARITY ON GTAW OF ALUMINUM
Erin Anderson
THE IMPORTANCE OF SAFETY AND THE IMPACT OF OSHA IN THE WORKPLACE
Ezra Huey
THE CARE OF LOW HYDROGEN ELECTRODES AND ITS IMPACT ON WELD QUALITY
Michael J. Herkert
Category C
SUPER DUPLEX STAINLESS STEEL: EFFECTS OF MULTI-PASS WELDING PARAMETERS ON MICROSTRUCTURAL STABILITY
Timothy Pickle and Peter Morriss
INVESTIGATION OF THE HARDENING RESPONSE OF PRECIPITATION HARDENED STAINLESS STEEL 17-4 DURING MULTI-PASS WELDING
Allison Fraser and Robert Hamlin
MANIPULATING MANUFACTURING VARIABLES WHEN SPOT WELDING HIGH STRENGTH STEEL STACK-UPS
Nick Colvin, Ethan Flathers and Alex Griffith
Category D
STRESS RELIEF CRACKING SUSCEPTIBILITY IN HIGH TEMPERATURE ALLOYS
Rishi Kant
EFFECT OF POWDER CONTAMINATION ON SELECTIVE LASER MELTED 17-4 PH STAINLESS STEEL
Devon Gonzales
PRINTABILITY OF ALLOYS FOR ADDITIVE MANUFACTURING
Tuhin Mukherjee
Category E
CHARACTERIZATION OF GRADED TRANSITION JOINTS FOR ENERGY APPLICATIONS
J. Galler
CHARACTERIZATION OF HOOK FORMATION IN FRICTION STIR WELDING AI/Fe DISSIMILAR METAL LAP JOINT
San Hoon Kang
HOT CRACKING SUSCEPTIBILITY OF Ni-Cr-Fe ALLOYS UTILIZING THE TRANS-VARESTRAINT TEST
Sangwoo Nam
2015 POSTER WINNERS
Category A
SPRAY TRANSFER VERSUS ADVANCED GMAW-P
Shane Markham
Category B
DISTORTION MODELING OF WHEEL LOADER ARTICULATION JOINT
Michael Orr and Jansen Lenzo
TOWARD FUNDAMENTAL UNDERSTANDING OF PECULIAR MAGNESIUM SEGREGATION DURING WELDING OF ADVANCED HIGH-STRENGTH ALUMINUM
Andrea Peer
REFILL FRICTION STIR SPOT WELDING MATERIAL STACK-UP ANALYSIS
Andrea J. Peer, Jacob J. Rindler and Mike Spodar
WAVEFORM COMPARISON BETWEEN STT, CV AND POWER MODE GMAW PROCESSES
Ryan Akers, Preston Anderson and Mike Barret
ULTRASONIC PLASTIC WELDING: JOINT COMPARISON FOR VALOX 325
Justin Wenning, John Parsons, Avraham Benatar and Miranda Marcus
Category C
MICROSTRUCTURAL EVOLUTION AND CREEP-RUPTURE BEHAVIOR OF A-USC ALLOY FUSION WELDS
Daniel Bechetti, John DuPont, John Shingledecker and John Siefert
PHASE TRANSFORMATIONS AND MECHANICAL PROPERTIES OF FUSION WELDS IN 10 wt% NICKEL STEEL
Erin Barrack and John DuPont
MICROSTRUCTURAL EVOLUTION AND MECHANICAL PROPERTIES OF SIMULATED HEAT AFFECTED ZONES IN CAST PRECIPITATION HARDENED STAINLESS STEELS 17-4 AND 13-8+MO
Robert Hamlin and John DuPont
IN-SITU STRAIN MEASUREMENT DURING ARC WELDING PROCESS USING DIGITAL IMAGE CORRELATION
Zongyao Chen, Jian Chen, Huabin Chen
FRICTION AND FUSION DISSIMILAR WELDING OF STAINLESS STEEL TO 1018 STEEL
Nathan Switzner, Zhenzhen Yu, Michael Eff, Arthur Fonseca and Stephen Liu
Category D
CORRELATIONS BETWEEN MICROSTRUCTURE AND PROPERTY OF FRICTION STIR WELDED JOINTS OF HIGH NITROGEN AUSTENITIC STEELS
Ruidong Fu, Dongxu Du, Yijun Li, Zhenzhen Yu
Category E
TURNING WELDING INTO MUSIC
Max Der Boghossian, Cory McIntosh and Patricio F. Mendez
TOUCH SENSING FOR ROBOTIC WELDING
Amanda Dubrule and Gentry Wood
2013 POSTER WINNERS
Category A
CARBON MIGRATION IN DISSIMILAR WELDS
Simon Rowe
BALLISTICS TESTING OF FSW 2050-T8 ALUMINUM-LITHIUM ALLOY
Michael Lannom, Jim Farrington and Brent Helmick
Category B
GRAIN REFINEMENT IN 52M FILLER METAL THROUGH ULTRA-SLOW CURRENT PULSING
Erik Birkinbine, Vernon Kreuter, and Nathan McVicker
GMAW TRANSFER MODE MONITOR
Joseph Russell, William Bunker, Stephanie Nystrom, Derek Hoyt and Nathan Berthiaume
EVALUATION OF AN ENHANCED FLUX CORED CONSUMABLE
Eric Przybylowicz, Derek Jones and Bryan Riggs
EFFECT WELDING VARIABLES ON POROSITY IN 2.5CR-1MO GMAW WIRES
Mary Bechie, Goran Lokas, Patrick Long and Timothy McGoughan
DEVELOPMENT OF A HIGHLY RELIABLE HOT ISOSTATIC PRESS CAN WELD
Cory O’Brien, Andrew Irwin and Jared Proegler
DESIGN OF PORTABLE FRICTION STIR WELDING SYSTEM AND THE
DEVELOPMENT OFACTIVE FEEDBACK CONTROLS
Bryan Patton, Sylvester Stafford and Clay Varner
Category D
INVESTIGATION OF TCHP SURFACE COATINGS FOR EXTENDED LIFE
Anita Hancox, John Keane and Dave Evans
2012 POSTER WINNERS
Category A
Steven Zeal, Jason Rhoton and Lam T. Lam
Category B
T.E. Borchers, M.E. Hahn, B.A. Lowiec and D.J. Tung
Jared Martin, Christopher Barnhill and Michael Presley
Timothy Bucher, Margaret Kittila and Joseph Steiner