A group of joining processes that produces coalescence of materials by heating them to the soldering temperature and by using a filler metal having a liquidus not exceeding 840 degrees Fahrenheit (450 degrees Centigrades) and below the solidus of the base metals. The filler metal is distributed between closely fitted faying surfaces of the joint by capilary action or by wetting the surfaces of the workpieces.
^