The fourth step of the preparation process for metallographic specimens. Polishing is similar to grinding, and is performed by rubbing the specimen with soft cloths treated with a special polishing powder. Specimens are polished in order to remove damaged layers that were not addressed by grinding, producing a smooth finish.