400 series steels chromium and nickel as their main alloying elements. Martensitic stainless steels have a BCT crystal structure, are magnetic, brittle, and can be heat treated. They can contain up to 1% carbon, and are generally less weldable and resistant to corrosion than austenitic stainless steels.
^