The third step of the preparation process for metallographic specimens. Grinding a specimen removes surface layers that were damaged from the sectioning process. This is performed, manually or mechanically, by rubbing the specimen with special abrasive paper. This process is repeated numerous times, using abrasive papers of increasing fineness.