Fillet Weld Size

For equal leg fillet welds, the leg lengths of the largest isosceles right angle that can be inscribed within the fillet weld cross section For unequal leg fillet welds, the leg lengths of the largest right triangle that can be inscribed within the fillet weld cross section.