This conference brought together the industry’s outstanding experts to discuss the welding of austenitic, duplex, and other grades of stainless steel. Topics included dissimilar metal welds between stainless and steel, repair welding, cladding, cleaning, and the pitfalls involved in stress corrosion cracking.
Please click on a link below to view the password protected PDF document
Conference Attendees
In order to acquire your password
PLEASE CONTACT
Martica Ventura at mventura@aws.org or 800 443-9353 x224
Repair Welding of Stainless Steels
by Frank Babish
An Update on AWS D1.6 Structural Welding Code
by Richard Campbell
Effect of Welding Variables on Duplex Stainless Steel Corrosion Resistance
by Gary Carinci
Process Analysis of Laser, Plasma, and Waterjet Cutting & Marking of Stainless Steel Sheet
by DeFalco
Innovations and Advancement in Metal Cored Stainless Steel
by Eckhardt
Orbital Welding of Stainless Steel
by T.E. Gittens
Stress Corrosion Cracking
by Grubb
Effect of SAW Parameters on Properties of Stainless Steel CROs and Qualification & Control of Weld Cladding for H2S Service
by Richard Holdren
Landmark Events in the Welding of Stainless Steels
by Damian Kotecki
Is There a Right Blend for Welding Stainless Steel
by Lyttle
Laser Based Deposition of Stainless Steel Alloys
by Rick Martukanitz
16-8-2 Utilizes Controlled Residual Elements to Enhance and Maintain Elevated Temperture Creep Strength
by William F. Newell
Explosion Welded Stainless Steel Cladding
by Jose Olivas
Insights into Passivation Welding & Rouge
by Daryl Roll
Dissimilar Metal Welding of the Austenitics to the Ferritic Steels
by Donald Tillack