Microstructural Characterization of Dissimilar Metal Cold Metal Transfer Weld Overlays


Researchers show how cold metal transfer produces structural weld overlays that are less susceptible to solidification cracking than those produced with GTAW.

One thought on “Microstructural Characterization of Dissimilar Metal Cold Metal Transfer Weld Overlays”

  1. Hi,

    I am currently working, for my master’s lab project, on dissimilar welding of duplex stainless steel to the austenitic 316 L. I am triyng to analyse the effect of robotic CMT parameters on the susceptibility to crater solidification cracking.

    My question is regarding the partion coefficient of Cr and Ni, which method have you used to program thermocalc calculator ? and did you correlated it with dilution based on composition gradient?

    Best regards