Super Duplex Stainless Steel Overlays in Electroslag Welding

Super Duplex Stainless Steel Overlays in Electroslag Welding

Researchers at Sandvik highlight the suitability of super-duplex stainless steels for corrosion resistant overlays deposited with conventional welding methods.