Tool and Preheat Coil Offset in Dissimilar Friction Stir Welding

Tool and Preheat Coil Offset in Dissimilar Friction Stir Welding

Researchers developed a method of offsetting the tool pin and preheat coil to predict the weldability of all dissimilar metal combinations with the FSWProcess.