Failure Analysis of Dissimilar Weld Joint on Transfer Line of Direct Reduction Steel Plant

Failure Analysis of Dissimilar Weld Joint on Transfer Line of Direct Reduction Steel Plant

Researchers at an iron reduction plant discuss circumferential cracking in a dissimilar weld involving a nickel chromium alloy and ASTM A106 Gr. B Tube.