Weld Metal Microfissuring in Fe-Ni-Co-Cr Alloy

Weld Metal Microfissuring in Fe-Ni-Co-Cr Alloy

Researchers used the GMAW process on HAYNES 556® alloy to determine the root cause of microfissures that lead to cracking in multipass welds.