Application of the Delayed Hydrogen Cracking Test

Effects of Welding Variables on the Weldability of High Manganese Steel

The results of delayed hydrogen cracking tests on dissimilar metal welds designed to solve the problem of brittle failures in subsea oil and gas piping.