Piping Erection Practice by FCAW-GS in Oil and Gas Industry

Piping Erection Practice by FCAW-GS in Oil and Gas Industry

In order to apply FCAW-GS to all-position welding of carbon steel piping in new plant construction in the oil and gas industry, suitable welding consumables and welding procedures were developed.